03 / Tools
A little less guesswork.
Small tools for the studio. Start with the numbers, see how they relate, and keep the assumptions in view.
Your estimate
Engineering estimate, not a validated kiln repair specification. Check element temperature, supports, surface loading and the electrical design independently.
Your starting size
Uses linear shrinkage measured relative to the wet dimension. Clay body, forming and firing affect the result: use a test bar for your own process.
Coil equations, assumptions & sources
One continuous, uniform active element at the voltage entered. No series/parallel bank conversion, lead resistance, contact losses, thermal expansion, springback or changing coil diameter during stretching is included. Stretched length is the ideal axial advance along the coil path; end effects are ignored. The resistance factor must match the alloy and element temperature, not simply the kiln air temperature.
A = πd²/4 · r = ρ/A · R20 = rL · Rt = CtR20 · I = V/Rt · P = V²/Rt
For target power: L = V²/(P × Ct × r). With wire length Lmm, stretched length S and mean diameter Dm = Di + d: N = √(Lmm² − S²)/(πDm); pitch p = S/N; clear gap p − d. Surface area in cm² is πdLmm/100.
The example follows dimensions in the kiln project's main README. Its published pitch expression uses outer minus inner diameter; this planner uses mean centreline diameter. With 21.5 m wire, 1.6 mm wire diameter, 8 mm inside diameter and 3648 mm stretched length, that gives about 5.2 mm pitch. The esphome branch still needs comparison.
Resistivity references: Kanthal D datasheet and Kanthal A-1 datasheet. No universal acceptable surface-load range is assumed.
Shrinkage equation
Wet size = finished size / (1 − shrinkage / 100). This is a linear-size calculation, not a volume calculation.